Lab 6- Non-Destructive Evaluation
Lab
Observation Radar Infrared Imaging Cover MeterFlatjack TestingImpact Echo Testing
Extras
Lab HandoutPhotosSample Results Sample Lab ReportLab Equipment and materialsExtra ResourcesLab WorksheetPrinter Friendly Version |
In-situ Test Results
Stress |
Gage Length |
0 |
8.00000 |
150 |
7.99880 |
200 |
7.99917 |
250 |
8.00020 |
300 |
8.00177 |
350 |
8.00300 |
400 |
8.00450 |
450 |
8.00610 |
500 |
8.00740 |
550 |
8.00877 |
600 |
8.01043 |
650 |
8.01167 |
700 |
8.01303 |
750 |
8.01460 |
800 |
8.01590 |
Deformation Test Results
Change in Stress |
Change in Strain |
0 |
0 |
53 |
0.00005 |
100 |
0.00009 |
150 |
0.00018 |
200 |
0.00024 |
250 |
0.00029 |
300 |
0.00036 |
350 |
0.00040 |
400 |
0.00042 |
450 |
0.00050 |
500 |
0.00054 |
550 |
0.00057 |
600 |
0.00060 |
650 |
0.00066 |
|